2021-01-292021-01-292013-07-05XII International Workshop on Plasma Based Ion Implantation and Deposition. Francia. (2013).http://hdl.handle.net/20.500.12272/4771In this work, AISI316L stainless steel was nitrided using three different processes: Low Energy Ion Implantation (LEII), Plasma Immersion Ion Implantation (PI3) and DC Pulsed Plasma Nitriding (DCPPN). The process temperature was chosen between 390 and 430 °C in all processes with the aim of preserving their corrosion resistance.application/pdfenginfo:eu-repo/semantics/openAccesshttp://creativecommons.org/licenses/by-nc-nd/4.0/Attribution-NonCommercial-NoDerivatives 4.0 InternacionalAISI 316LStainless steelComparison of wear and corrosion behavior of three different nitriding methods on AISI 316L stainless steelinfo:eu-repo/semantics/conferenceObjectDalibón Bähler, Eugenia Laura ; Vaca, Laura Silvia ; Brühl, Sonia Patricia ; Escalada, Lisandro ; Simison, Silvia ; Manova, Darina ; Mändl, Stephan ; Neumann, HorstNo comercial con fines académicos.