Abstract
In this work, AISI316L stainless steel was nitrided using three different processes: Low Energy Ion Implantation (LEII), Plasma Immersion Ion Implantation (PI3) and DC Pulsed Plasma Nitriding (DCPPN). The process temperature was chosen between 390 and 430 °C in all processes with the aim of preserving their corrosion resistance.